Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3EG7 FC Aqua BK23285 - PA66-GF35 - BASF

Material Data Center offers the following functions for Ultramid® A3EG7 FC Aqua BK23285:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Ultramid® A3EG7FC Aqua black 23285 is optimized for plastic parts, mandatory requiring material approvals for drinking water or direct food contact
The product is approved according to
• 21 CFR FDA § 177.1500 "Nylon resins" (for repeated use applications only)
• 21 CFR FDA § 178.3297 "Colorants for polymers” (for repeated use applications only)
• European Food Contact European Food Contact Commission Regulation (EU) 10/2011
• GMP (EC) n°2023/2006

and provides the approvals for drinking water regulations of

• KTW
• DVGW W270
• WRAS
• ACS (disclosure of ingredients)
• NSF (disclosure of ingredients)

For questions regarding the compliance with further regulations, and certificates, please contact your local BASF representative or Plastics Safety (E-Mail: plastics.safety@basf.com).
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 30 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
Contracción posterior al moldeo, paralelo 0.4 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.0 / * % ISO 294-4, 2577
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 11500 / 8500 MPa ISO 527
Resistencia a la tracción 210 / 150 MPa ISO 527
Alargamiento a rotura 3 / 5 % ISO 527
Módulo de plastodeformación, 1000h * / 6650 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C 95 / 105 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 75 / - kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 14 / 22 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 12 / - kJ/m² ISO 179/1eA
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 260 / * °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 250 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 250 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 250 / * °C ISO 306
Coef.de expansión térmica lineal, paralelo 17.5 / * E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 65 / * E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.6 / * mm -
Yellow Card disponible sí / * - -
Combustibilidad a espesor h HB / * class IEC 60695-11-10
Espesores de probeta 0.8 / * mm -
Yellow Card disponible sí / * - -
Combustibilidad según índice de oxigeno 24 / * % ISO 4589-1/-2
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 1MHz 3.5 / 5.7 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 200 / 3000 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 200 / 1500 E-4 IEC 62631-2-1
Resistividad volumétrica específica 1E13 / 1E10 Ohm*m IEC 62631-3-1
Resistividad superficial específica * / 1E10 Ohm IEC 62631-3-2
Resistencia dieléctrica 39 / 37 kV/mm IEC 60243-1
Indice comparativo de linea de fuga - / 550 - IEC 60112
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 5 / * % Sim. to ISO 62
Absorción de humedad 1.6 / * % Sim. to ISO 62
Densidad 1410 / - kg/m³ ISO 1183
Propiedades específicas del materialSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de viscosidad 145 / * cm³/g ISO 307, 1157, 1628
Funciones
Viscosidad-velocidad de cizallamiento , Ultramid® A3EG7 FC Aqua BK23285, PA66-GF35, BASF
Tensión de cizalla-velocidad de cizalla , Ultramid® A3EG7 FC Aqua BK23285, PA66-GF35, BASF
Módulo de cizallamiento dinámico-temperatura , Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Módulo de cizallamiento dinámico-temperatura , Ultramid® A3EG7 FC Aqua BK23285 (Cond), PA66-GF35, BASF
Esfuerzo-alargamiento , Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Esfuerzo-alargamiento , Ultramid® A3EG7 FC Aqua BK23285 (Cond), PA66-GF35, BASF
Módulo secante-alargamiento , Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Módulo secante-alargamiento , Ultramid® A3EG7 FC Aqua BK23285 (Cond), PA66-GF35, BASF
Esfuerzo-alargamiento (isocrono) 23°C, Ultramid® A3EG7 FC Aqua BK23285 (Cond), PA66-GF35, BASF
Módulo de plastodeformación-tiempo 23°C, Ultramid® A3EG7 FC Aqua BK23285 (Cond), PA66-GF35, BASF
Curva de creep 23°C, Ultramid® A3EG7 FC Aqua BK23285 (Cond), PA66-GF35, BASF
Esfuerzo-alargamiento (isocrono) 60°C, Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Módulo de plastodeformación-tiempo 60°C, Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Curva de creep 60°C, Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Esfuerzo-alargamiento (isocrono) 90°C, Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Módulo de plastodeformación-tiempo 90°C, Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Curva de creep 90°C, Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Esfuerzo-alargamiento (isocrono) 120°C, Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Módulo de plastodeformación-tiempo 120°C, Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Curva de creep 120°C, Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Esfuerzo-alargamiento (isocrono) 140°C, Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Módulo de plastodeformación-tiempo 140°C, Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Curva de creep 140°C, Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Volumen especifico-temperatura (pvT) , Ultramid® A3EG7 FC Aqua BK23285, PA66-GF35, BASF
Módulo a tensión-temperatura , Ultramid® A3EG7 FC Aqua BK23285 (Seco), PA66-GF35, BASF
Módulo a tensión-temperatura , Ultramid® A3EG7 FC Aqua BK23285 (Cond), PA66-GF35, BASF
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola, Negro
Aditivos
Lubricante, Desmoldeante
Características especiales
Estable contra el calor
Certifications
Contacto con alimentos, Aprobación a contacto con alimentos 10/2011, Aprobado por el FDA 21 CFR, Contacto con agua potable, Contacto con agua potable KTW, Contacto con agua potable DVGW W270, Contacto con agua potable NSF 61
Disponibilidad regional
Demás información
Moldeo por inyección
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 280 - 300 °C
injection molding, Melt temperature, recommended: 290 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.